Pulp Production

  • Worn internals of hydropulper.  Severe wear can cause rupture of vessel.

  • Final surface after ARC®  890 was applied.  First evaluation showed no wear present.

  • Hydropulper base was tack welded with expanded metal mesh, abrasive blasted and solvent cleaned with ARC 203.

  • 286 kg of ARC® 890 was applied.